Austin Club Plus

STRUCTURAL BLOCKBOARD

Lorem ipsum dolor sit amet consectetur, adipisicing elit. Itaque accusantium odio optio nemo doloribus reiciendis nihil. Delectus eum odit, odio dolores perferendis itaque. Expedita, eos asperiores, dolores dolorum ratione, exercitationem blanditiis est vero error modi et cumque quam impedit fuga!. Lorem ipsum dolor sit amet consectetur adipisicing elit. Fuga qui soluta explicabo facere tenetur corporis tempora ratione. Veritatis, nihil eveniet.

single_project
  • 100% High Quality Meghalayan Pine Wood.
  • 500 % Lifetime warranty.
  • Boiling Water Proof.
  • E1 Emission Level.
  • Quadruple Pressed. ( Two times Pre-pressing and two times Hot Pressing).
  • Double Calibrated for uniform thickness.
  • 3-Tier Preservative Treatment : Pressure impregnation treated fillers, GLP and Full Cell ACC ( Acid copper Chrome).
  • Bonded with un extended phenol Formaldehyde Resin of BWP Grade.
  • Strictly follow Pre-pressing Technique. Pre-Pressing ensures sufficient time for transferring of wood preservative in each and every particles of veneer before Hot Pressing. It helps in distribution of moistureand adhesive more uniformly to make the plywood more strong , durable and free from warping, twisting and cupping.

TECHNICAL SPECIFICATIONS

  • Dimension and Tolerance
    • Length, mm : +2mm, 0mm
    • Width, mm : +1mm, 0mm
    • Thickness below 6mm, % : +2.5%
    • Variation in Thickness, mm : 0.3
    • Squareness, % : 0.08%
    • Edge Straigntness, % : 0.09%
  • Workmanship & Finish : Satisfactory
  • Dimensional changes caused by humidity, N/mm^2
    • Changes in Length From 65 % RH to 90 % RH, mm : +0.2
    • Changes in Length From 65 % RH to 40 % RH, mm : -0.15
    • Changes in width From 65 % RH to 90 % RH, mm : +0.08
    • Changes in width From 65 % RH to 40 % RH, mm : -0.06
    • Local Planeness : <1/210
    • At the extreme range of Humidity : No Delamination
  • Adhesion of Plies ( Knife Test ) : Execellent
  • Resistance to Water (60±2℃) : Execellent
  • Registance to Micro organism : No sign of seperation
  • Modulus of Elasticity, (N/mm²)
    • Average : 6250
    • Minimum Individual : 5500
  • Modulus of Rupture, (N/mm²)
    • Average : 61.75
    • Minimum Individual : 56.45
  • Spoil Test : Treated